6G welding test with tig root pass on a 3" XXH wall, with a full tig welding procedure.
6G is where the pipe is fixed at a 45-degree angle and welded in this fixed position.
So, it basically covers flat, horizontal, vertical welding, and overhead in a single position.
In this video, I will break down the steps to pass the 6G position test, starting with the root pass, and in the second video, I will show the steps from fill passes to finish with a multi-pass cap.
The pipe welding techniques used, and the welding procedure is also identical to the AWS D1.1 and ASME Section IX welder performance qualification (WPQ) pipe welding certification. As per ASME Section IX.
#tig #tigwelding #rootpass
All of my videos are recorded at working sites in various locations and different welding positions.
90% of my welding projects in videos are x-rayed, and if you like to see hands-on projects, welcome!
If you liked this video please give it a thumbs up, share it, subscribe and click the bell.