Aluminum etching with ferric chloride. 

Matěj Novák
Подписаться 3,2 тыс.
Просмотров 160 тыс.
50% 1

When etching generates heat and fumes. Therefore, ventilate the room where you work.
Etch 30 seconds to 1 minute after the aluminum plate put into cold water to cool, tooth brush gently clean the etched surface and give another etch. Repeat this process until etched surface will have the desired depth.

Опубликовано:

 

24 авг 2024

Поделиться:

Ссылка:

Скачать:

Готовим ссылку...

Добавить в:

Мой плейлист
Посмотреть позже
Комментарии : 155   
@khokanmanna5475
@khokanmanna5475 2 года назад
Engraved is doing ,but no deep by ferric chloride , ans. & slove my problems pls sir ,
@EssexSilvering
@EssexSilvering 5 лет назад
One word ................ Brilliant!!
@samirpasic6836
@samirpasic6836 5 лет назад
Nice video Can you tell me ,can i do the same etching with electricity and salt water on aluminum like yours ??? And can you tell me how many times I can use the same ferric chloride??? Thank you
@davidhorsley1149
@davidhorsley1149 Год назад
Hydrochloric acid (Muriatic Acid) will also etch aluminum. You just have to thoroughly neutralize it afterward.
@Splatterpunk_OldNewYork
@Splatterpunk_OldNewYork 5 лет назад
So you are yanking the aluminum plate out of the ferric chloride bath every minute because it gets hot from the reaction. You are cooling the thing in cold water and scrubbing the left over gunk with a toothbrush, then repeating the process. I was wondering if this method is suitable for delicate intaglio etching on aluminum that is much thinner. Guess I will see. My only worry is the asphaltum resist I am using might fail if temp is an issue. Wondering if some good old enamel lacquer might do the trick instead.
@arhalimi5883
@arhalimi5883 6 лет назад
.. one of the best time lapse vids i hv come across & of coz the OMG a fantastic etching work .. could hv added sub for info of the processes .. neway, tQ.
@mdrafiuddiniquabal291
@mdrafiuddiniquabal291 3 года назад
Please say what is name of polishing device and company. Thax.
@meeseeks4795
@meeseeks4795 Год назад
At 3:15 did anyone else hear the Pokémon random battle sound on gba? Lol
@rubenmanzione
@rubenmanzione Год назад
Hola estás grabando una placa de aluminio??? Cuánto tiempo de inmersión en cloruro férrico???muchas gracias muy buen trabajo!!!!
@moeezhusainbadshah83
@moeezhusainbadshah83 4 года назад
nice job
@making-arte5710
@making-arte5710 3 года назад
Your job is awesome !!! :O Thanks for the video x) Its really great !!! :D What kind of paper do you use? :o
@jefflockwood3421
@jefflockwood3421 7 лет назад
Awesome video, thank you!!! One question I have as I'm trying to figure out the best way to do a project similar to yours is what materials are you using to create the transfer? Also it looks like your using simple packing tape on the back to prevent etching?
7 лет назад
To transfer the image I use "transfer foil for vinyl cut graphics" But I'm not sure if this is the exact translation. I have a foil from graphic studio where I let cut out the stickers. For covering the back side you can use any tape. It is there purely to seal the surface is not etched.
@PaulHaggar
@PaulHaggar 3 года назад
Sound of fast forwarding is terrible. I recommend cutting the audio out or do some explanation of what you’re doing and the products you use. This is not really a tutorial as much it is you showing off what you can do. Nice job though on the sign.
@chrinamint
@chrinamint Год назад
I think it's kind of cool. Perhaps you could just mute it.
@PaulHaggar
@PaulHaggar Год назад
@@chrinamint wish I could do the same for you… alas it’s the internet and stupidity is expected.
@chrinamint
@chrinamint Год назад
@@PaulHaggar LOL!
@andrewgray9663
@andrewgray9663 Год назад
The title doesn't say it's a tutorial although that's what I was looking for. Still found this helpful although it would be useful to have details of the chemicals involved.
@PaulHaggar
@PaulHaggar Год назад
@@andrewgray9663 I agree, would have been nice to get a description of materials used. Cheers
@panglimaempatlima6631
@panglimaempatlima6631 4 года назад
Nice From INDONESIA
@sahilkhunger1001
@sahilkhunger1001 5 лет назад
hlo dear your video is so nice. but i have 1 question with you and my question is Can we reuse ferric chloride? if we can so how many time we can use? please help me dear i want to start this work I hope you rply me as soon as possible thnks dear
5 лет назад
Hi . This is not what we can say in general. When etching smaller items, chloride can be used several times. When etching bigger items, life is shortened.
@Kemalfrostfire
@Kemalfrostfire 4 года назад
Nice
@princekharlespartero1561
@princekharlespartero1561 Год назад
Hi..what are the components of the chemical..tnx
@dickwhittington7321
@dickwhittington7321 5 лет назад
Ferric chloride works faster if its heated up the the microwave for 20 seconds or so. Also use metal polish afterwards on the sanded aluminium, make it shine like a mirror.
@kdrama4754
@kdrama4754 2 года назад
If i use hot water its same?
@bhaskarbonala4226
@bhaskarbonala4226 2 года назад
Hi sir ferric chloride can eatinching Steel name plate
@CharlesEakins
@CharlesEakins Год назад
Great video, what is the black stuff you used?
@aphexnet
@aphexnet 5 лет назад
Nice work!!!!!
@utrejch-9389
@utrejch-9389 5 лет назад
Parada! Uplne cumim, jak se v domacich podminkach da vyrobit profesionalne vypadajici cedule! Vyborna prace! Dotaz: pokud by cedule byla venku, mas nejake doporuceni pro vrchni bezbarvy lak? Aby se na povrchu nedelala takova ta skareda šedá vrstvicka oxidu. Diky.
5 лет назад
Ahoj . Dělal jsem takhle jmenovky na domovní zvonek . Použil jsem nato barvy motip . A barvy vpohodě drží .
@SHINdanny
@SHINdanny 3 года назад
great video about a dot, that is supposed to be there but it is not and then magically appears_the MAGIC DOT
@adnansiddiq5582
@adnansiddiq5582 6 лет назад
Great Work.
@sreejiths3138
@sreejiths3138 5 лет назад
Which grade aluminium sheet is used... can use this metal nameboard for outside, all whether...? Pls help
5 лет назад
Hi . I made it out of duralumin. I don't know the alloy designation, I found it in the scrap. This procedure will work with any aluminum alloy. Yes the sign can be used outdoors. Similarly, I made name badges for the doorbell.
@user-xw3xr8yg3v
@user-xw3xr8yg3v 8 месяцев назад
If I don't have ferric chloride, can I use HCL acid with H202?
@regularhumanbeing5211
@regularhumanbeing5211 4 года назад
what is that stencil you are using? how did you get it made? It sticks to metals really well or what? I am trying to do that same thing and the only solution i came up with is to get some vinyl and a vinyl cutter...
@bittoodhiman7634
@bittoodhiman7634 4 года назад
good job brother 👍🌹
@CoolDude-ip9no
@CoolDude-ip9no 5 лет назад
wow, great work, bruh...thank u for sharing 😃👌
@baljazz
@baljazz 4 года назад
Would you be able to use a 3d print as a resist in order to save material? Or maybe wood. Not sure if it will eat through it. Trying to etch .25 inch stainless steel using the salt water electro etching method. Thanks.
@RockDog101
@RockDog101 5 лет назад
Very cool!
@butchcoplin2316
@butchcoplin2316 5 лет назад
That's fucking awesome
@VoidedWarranty
@VoidedWarranty Год назад
what was the music in the background at the end?
@gprice1978
@gprice1978 3 года назад
Awesome
@scienceandtechnologyst8134
@scienceandtechnologyst8134 2 года назад
Could you suggest me a video of making good and effective ferric chloride because I think my ferric chloride is not working well because it's not giving texture every where and not giving same texture as your gives .... kindly suggest me good video for making ferric chloride ...
@123Patrick
@123Patrick 4 года назад
Was that a vinyl or laser copy transfer.
4 года назад
vinyl transfer
@saviorebera8716
@saviorebera8716 Год назад
What's the chemical that you are using
@tngryf1234561
@tngryf1234561 2 года назад
Very nice. Thanks
@jayswartzfeger6723
@jayswartzfeger6723 4 месяца назад
nice work video too fast
@ahmedatef6683
@ahmedatef6683 4 года назад
What is the liquid used in timer 5:05? Great work by the way
@vespadano1979
@vespadano1979 4 года назад
Ahmed Atef It’s called dihydrogen monoxide.
@fernandosergio8450
@fernandosergio8450 4 года назад
kkkk.... I can't believe I google it...
@adinshankar7549
@adinshankar7549 4 года назад
Yes, It is known as H2O
@pistolgrip44mag
@pistolgrip44mag 5 лет назад
Very Cool
@karimgaddi3306
@karimgaddi3306 Год назад
How to use itching chemical
@jaybirdvc15
@jaybirdvc15 3 года назад
Dope
@jaimaadurga8412
@jaimaadurga8412 5 лет назад
Hi, nice work. Quite helpful. Tell me about stencil. Can it be made from vinyl sheets or is it some other material.
5 лет назад
Hi . I'm sorry I'm writing late. Yes, you can use vinyl. The template was made by an advertising agency for me. It's called "Cut Graphics".
@jamsheedkhan7513
@jamsheedkhan7513 2 года назад
Zara dhang se vidio banaiye janab ye kaya sarcas ke kartab dikha rhe ho
@adnansiddiq5582
@adnansiddiq5582 6 лет назад
Kindly tell me what kind of Black Ink. P.P or P.V.C.
@peterking2651
@peterking2651 4 года назад
Ok, but how do you get to part 1?
4 года назад
First part ? This is all. I put the sticker into an advertising agency. It's a vinyl sticker that makes car stickers.
@shabiayub3147
@shabiayub3147 6 лет назад
How to use etching chemicals
@noa2012prints
@noa2012prints 5 лет назад
Нi man.Can i ask how to remove wasting material/thrash/rust from plate?
5 лет назад
Hi, I use an old toothbrush.
@artjar1000
@artjar1000 7 лет назад
you rock Matej! can you help me with some details: how long did you leave it in ferric chloride?, why did you rinse it several times?, what paint did you use? and what solution did you use for cleaning the paint from the untouched surfaces?
7 лет назад
Thanks pleased me your interest. I let it etch 30-60 seconds. Then it rinse with clean water. Rinse with it due cooling because heat is generated during etching. And on the surface of iron settles, it will remove tooth brush so that the etched surface was not bumps. I am using plain color spray paint. To remove color using water sandpaper, grit 280.
@algorhythminc
@algorhythminc 2 года назад
@ how long do you wait for paint to dry before sanding down with water?
@ChetanSharma-mc5kr
@ChetanSharma-mc5kr 6 лет назад
Nice work, amazing combination of arts and science. Can electric circuits be prepared by etching process too??
6 лет назад
Yes, it is possible. But better results are achieved using a photosensitive lacquer. watch this video ru-vid.com/video/%D0%B2%D0%B8%D0%B4%D0%B5%D0%BE-9PXHXAArKaw.html
@drakkaritshan6273
@drakkaritshan6273 7 лет назад
Hello Matěj at the end you paint with spray and remove the ink using which product, grateful.
7 лет назад
To remove spray paint using water sandpaper, grit 280. Then another 500 grit for super-smooth finish.
@barrythornton9947
@barrythornton9947 6 лет назад
After spray painting... you poured something on from a can ? then sanded with wet n dry. What did you put onto the paint?
6 лет назад
That's pure water. I used sandpaper for underwater grinding.
@enidoku213
@enidoku213 5 лет назад
big like
@Steverobbo
@Steverobbo 5 лет назад
So I tried this today with a small 32mm diameter aluminium disc that was 2mm thick. I cleaned it with acetone first then sat it in ferric chloride but it didn't seem to bubble like that and doesn't seem to have done much. What have I done wrong.
5 лет назад
Hi . Did you use pure aluminum or anodized? If the surface of the aluminum is anodised it is not possible to etching.
@Steverobbo
@Steverobbo 5 лет назад
Matěj Novák I thought it was just pure aluminium but maybe it did have a coating of some kind on it. I never sanded over it first as I thought it was just clean aluminium. Maybe next time I will try that first. It has etched it a little bit but it took all day and didn't look close to the effect you got with yours. My ferric chloride says 40% is that strong enough.
5 лет назад
Yes it is possible that there was some coating on aluminum. The etching of pure aluminum takes place quite quickly. The chloride concentration you use is good. Try clean aluminum and it will work.
@brandonlowe7808
@brandonlowe7808 4 года назад
Was this piece of aluminum anodized? Also would ferric chloride affect the results if I used a vinyl stencil? I am wanting to do the chrome strips on the side of my truck but im not sure if it will work and Its hard to find intact aluminum pieces for a 73 shortbed f100
4 года назад
Sorry i'm late. aluminum must be clean. If aluminum is anodized it will not work. The chloride template does not affect the template. However, care should be taken for temperature and thin or sharp shapes. They tend to peel off.
@wtjewelry387
@wtjewelry387 6 лет назад
Hi what stencil did you use. .or what specific name for that transfer paper
6 лет назад
Hello . At the local graphic studio I made a template. Transfer film was included. These are common things.
@lacossanostra
@lacossanostra 9 месяцев назад
next time use some acetone to remove the sticker just put it in a layer of aceton and the sticker will desolve from the alu plate
@Hady_septirah313
@Hady_septirah313 2 года назад
does the etching time affect the etching depth
@hayden8486
@hayden8486 Год назад
Yes
@dennyibesibestech8015
@dennyibesibestech8015 5 лет назад
tembak pake mesin grafir.. lebih cepatt
@jmprinting2041
@jmprinting2041 5 лет назад
Good day sir ,what kind of sticker you use ?
5 лет назад
It is not a special sticker. It could be something like that .https: //www.alibaba.com/product-detail/3m-vinyl-sticker-color-die-cut_60332848970.html
@janokarpi
@janokarpi 5 лет назад
Zdravím, kde se dají nechat vyrobit ty "vyřezané" samolepky. Případně na koho by se měl obrátit. Děkuji
5 лет назад
Ahoj . Měli by to umět asi v každý reklamní agentuře . Dělají se s tím reklamní polepy na auta . Jmenuje se to řezaná grafika .
@a4ajit
@a4ajit 5 лет назад
Hi, I tried on aluminum but it took almost 10 min for 0.30mm dip etching. What should be concentration of FECL3? What’s etching process for Stainless Steel of different grades?
5 лет назад
Hello . 0.3 mm in 10 minutes is normal. I do not know the concentration of ferric chloride, I buy the finished mixed solution. For etching stainless steel try Electrolysis. Batteries and salt water. But I do not know if it will work I did not try it.
@a4ajit
@a4ajit 5 лет назад
Thanks sir
@chrinamint
@chrinamint Год назад
@@a4ajit I etch stainless steel all the time with ferric chloride. Same process this guy used. I cut a stencil and put the ferric chloride on there anywhere from 10 to 15 minutes. Then I put baking soda on it to stop the reaction and then wash it with water. I don't paint mine after though.
@omdhori
@omdhori 2 года назад
Mantap gan luar biasa
@drakkaritshan6273
@drakkaritshan6273 7 лет назад
Greetings this aluminum is stainless steel?
7 лет назад
This is a sheet of aluminum.
@drakkaritshan6273
@drakkaritshan6273 7 лет назад
I tried to corrode aluminum and it boiled
@kishoooooooooooo
@kishoooooooooooo 6 лет назад
should i heat the chloride ? because it changed the color only , what can i do ???
6 лет назад
No . Do not heat ferric chloride. Etching would take place very quickly. Chloride should have room temperature. The etching heats itself
@kishoooooooooooo
@kishoooooooooooo 6 лет назад
yes i'am done thank you dude but i waiting more videos
6 лет назад
Soon, there will be a new video. :)
@ssmith7100
@ssmith7100 7 лет назад
What is ferric chloride used for in the house hold?
7 лет назад
Occasionally etching printed circuit boards. Ferric chloride that can not be used for copper etching is used for etching aluminum.
7 лет назад
I'm sorry I probably wrote it vaguely. I use the same iron chloride for both copper and aluminum. Ferric chloride is capable of etching a certain amount of copper, and then copper is incapable of etching. This (used) ferric chloride is then used for etching aluminum.
@MySpace662
@MySpace662 6 лет назад
This is a Charley Chaplin Video, with a Keystone Corp.
@opsharma9185
@opsharma9185 6 лет назад
I want traning
@650tonyd
@650tonyd 7 лет назад
ferric chloride? did you dip it in water and baking soda to stop the process before you re-etch?
7 лет назад
To cool down and stop etching. Soak the aluminum plate only into clean water . I do not use baking powder.
@marbleartmathura448
@marbleartmathura448 6 лет назад
TonydlP650 8273676747
@user-vc5rp7nf8f
@user-vc5rp7nf8f 6 лет назад
no help at all. what materials did you use, how long did you do each step for... etc
6 лет назад
check out the video comments. everything is written there
@zohaibmughal8253
@zohaibmughal8253 6 лет назад
i want etching on round shape aluminum.deep 1mm so please give me any process for this work
6 лет назад
On the video to see it all. What do you not understand ?
@akbarkhan-dh5jt
@akbarkhan-dh5jt Год назад
Hlo sir
@samirpasic6836
@samirpasic6836 6 лет назад
Can you post link where you buy your Ferric chloride?? And wht is the best deal?
6 лет назад
Hello . Ferric chloride I buy in a local store. Here is the link but I do not know if it will help you. www.gme.cz/leptaci-roztok-1000ml
@samirpasic6836
@samirpasic6836 6 лет назад
Do you have fb,i have some questions,thank you
6 лет назад
I only have a private Facebook. Please write your questions here. Thanks
@samirpasic6836
@samirpasic6836 6 лет назад
How thick is your alumin sheet,and how many times you can use the same ferric chloride solution???
6 лет назад
The minimum thickness of the aluminum plate is about 1 cm. I used a 2mm thick plate. I can not say how many times the same solution can be used. It always depends on how large the surface you are etching. Logo JD what is in the video could be etched about 5 times.
@noa2012prints
@noa2012prints 7 лет назад
great work,is this plate can used for printing?
7 лет назад
Hello . Do you mean to use it as a printing master? Maybe yes, but I have not tried it. Etched surfaces are deep cca.0,15mm.
@noa2012prints
@noa2012prints 7 лет назад
Tanx a lot for information.Just one more question,how long time i need for this deep?
7 лет назад
Time etching can not say exactly. Heat is created during etching. Larger etched surface creates more heat. And the warmed etching bath. How bath has higher temperature by the aluminum etches faster. Etch 30 seconds to 1 minute after the aluminum plate put into cold water to cool, tooth brush gently clean the etched surface and give another etch. Repeat this process until etched surface will have the desired depth. I repeated this about 6 times me to get to the depth of 0.15 mm.
@noa2012prints
@noa2012prints 7 лет назад
Many tanx for information and help.I will write it soon. Tanx again.You are great.
7 лет назад
you're welcome
@sz6182
@sz6182 2 года назад
The background sound is infuriatingly obnoxious.. Couldn’t watch more than 30 seconds sorry.. I’m sure it was good, but F that noise ✌️
@arissehasen7383
@arissehasen7383 Год назад
Bb
@KpxUrz5745
@KpxUrz5745 2 года назад
Despite the demonstration, it wasn't clear just what the steps are.
@drakkaritshan6273
@drakkaritshan6273 7 лет назад
Not good like yours.
7 лет назад
Aluminum must not be immersed in ferric chloride for too long. Otherwise, it will overheat and bath starts to foam. Aluminum immerse in chloride for a maximum of 30s. Then rinse in cold water and immerse again in chloride. Repeat it until the pattern is etched deep enough.
@drakkaritshan6273
@drakkaritshan6273 7 лет назад
t was then that happened because I'm looking for a way to make a deep solder in the metal, I got the copper and the brass but I wanted something even deeper, I saw some techniques with salt and vinegar using 12v batter and pile too, thank you.
7 лет назад
Etched with salt, vinegar and 12V battery I did not try. I can not help you with that.
@drakkaritshan6273
@drakkaritshan6273 7 лет назад
I'll put a lemon juice conentrado with the salt in the battery because the salt corrodes too and I'll come back to tell you the result, thank you
7 лет назад
George Robartes: What fish and chips? I do not understand....
@marteejadev.forelo4814
@marteejadev.forelo4814 7 лет назад
WRONG ETCHANT SOLUTION....
7 лет назад
Maybe yes but it works.
@danique1254
@danique1254 3 года назад
Niceee
Далее
Acid Etching Aluminum for Custom Nameplates
8:24
Просмотров 295 тыс.
How to Etch Aluminum / Etched Guitar Pedals
7:35
Просмотров 62 тыс.
Etching Brass With Ferric Chloride
5:28
Просмотров 39 тыс.
Simple Aluminum Etching with sticker | BIJU ART TECH
10:32
Drawing on metal. Anyone can repeat this.
7:25
Просмотров 423 тыс.
A glimpse into my etching process
8:11
Просмотров 63 тыс.
SIMPLE tech. Battery draws on metal
9:15
Просмотров 16 млн
Etching Aluminum Name Plates
5:45
Просмотров 129 тыс.