Тёмный

Chrome Plating Process I Gadhia Agencies I REDOX REATION PVT. LTD. RAJKOT 

Blue Planet Design Studio
Подписаться 54 тыс.
Просмотров 212 тыс.
50% 1

Chrome Plating plant manufacturer
GADHIA AGENCIES - SINCE 1967
RAJKOT (GUJARAT) INDIA.
EMAIL : sunil.gadhia@yahoo.com
Geet Gadhia : +91 98986 22616
Sunil Gadhia : +91 98797 42116

Кино

Опубликовано:

 

24 июл 2020

Поделиться:

Ссылка:

Скачать:

Готовим ссылку...

Добавить в:

Мой плейлист
Посмотреть позже
Комментарии : 88   
@jeetendrasinghchauhan3725
@jeetendrasinghchauhan3725 2 года назад
Good plant layout and presentations. Good Luck 💐💐💐💐💐💐
@professorbnelson3592
@professorbnelson3592 3 года назад
Thank you for sharing this video. A very clear demonstration of your plating line at work. Will be interesting for my Process Quality Engineering class for International students in Canada.
@sunilgadhia2458
@sunilgadhia2458 3 года назад
Thank you so much...Sir For your valuable feedback
@Solace037
@Solace037 3 года назад
This a great video. But what are they doin? Do they know what they are doin. It irritates me seeing people trained by someone who says "put it here 30s then rinse then this tank 45s.." Explain why and the chemical reaction thats happening.
@umarussemanda2894
@umarussemanda2894 2 года назад
@@sunilgadhia2458 I wish to get more information from you Sir
@John-un3lj
@John-un3lj 3 года назад
Very nice step by step video.
@adilyounas1987
@adilyounas1987 3 года назад
Very informative ..... Nice work
@jenniferdomingo28
@jenniferdomingo28 2 года назад
Very nice good job..I like the Job..
@BondanHeru
@BondanHeru 2 года назад
Clear well work presentation
@mruneek
@mruneek 2 года назад
Im a aerospace technician platter and yes wear your gear at all times 👨‍🔬
@PooleySteen
@PooleySteen Год назад
Typically, what types of quality control methods of chemical analysis of the bath are used to optimise the process?
@prankulluck
@prankulluck 2 года назад
Plz mention the process sequence and dipping time and jig design with example.
@PK-lc4fx
@PK-lc4fx 2 года назад
nice video 👍👍👍
@manjeshkumarsrivastav2780
@manjeshkumarsrivastav2780 3 года назад
Yes right work mai bhi yahi kaam karta hu
@manjeshkumarsrivastav2780
@manjeshkumarsrivastav2780 2 года назад
@Jha ,,entertainment 😊 hello
@abboudboudrama8071
@abboudboudrama8071 2 года назад
Je suis surpris par simplicité de ce procéder et j'aimerai beaucoup avoir. une petite installation comme Ça seulement il me. fat beaucoup d'aide par exemple. ou je je peu m'approvisionner de produits ou je peu trouver les bacs ect...
@vasaveliyasandip7587
@vasaveliyasandip7587 3 года назад
You are do the electropolishing process in your company.. Plese share contact details of new development whole the process of electropolishing..
@jenniferdomingo28
@jenniferdomingo28 2 года назад
Ganyan ang work q s dai ichi all around ako s plating in 10 years..kya lng wla n ako work
@alfieatienza3589
@alfieatienza3589 3 года назад
I experience in taiwan but no fully hightech more on man power☺️☺️
@mohdahmad3489
@mohdahmad3489 3 года назад
Nice
@mehfoozahmad651
@mehfoozahmad651 3 года назад
Very good plating
@mehfoozahmad651
@mehfoozahmad651 3 года назад
Sir please phone 📞 no sent
@QianaZianSTORY
@QianaZianSTORY 3 года назад
Without respirator😁
@roneystapes
@roneystapes 2 года назад
Little splash in your eye hurt nobody either 😂😂😂
@taherelassal4241
@taherelassal4241 8 месяцев назад
👌👌👌👌
@sudhirchauhanthakur8223
@sudhirchauhanthakur8223 2 года назад
Bhai ek video aisi bhi bana do is chemical par iske Karran humare kapde phat jate hai pls 🙏🙏🙏🙏🙏🙏🙏🙏
@adilyounas1987
@adilyounas1987 3 года назад
Specially sulfuric acid etching
@yoinkling
@yoinkling 3 года назад
Here from Clint's challenge
@joepetelo1839
@joepetelo1839 3 года назад
Nice setup
@flamingo6830
@flamingo6830 2 года назад
Exposure to chemical fumes is deadly
@rudrakshaaikar863
@rudrakshaaikar863 2 года назад
Please suggest how to make nickel plating dull if it's to much shiny
@debarghyahalder4653
@debarghyahalder4653 2 года назад
A carbon treatment will make the plating dull if you have added excess of brightener .. if you want a matte finish ...check the pH of the solution and adjust the pH to as low as 3.8 with help of sulfuric acid addition gradually.... It will give you a matte finish. Increase the additive levels more and not the brightener level
@jailaxmimarketing4235
@jailaxmimarketing4235 3 года назад
Need to know about full setup and their details.
@sahilKhan-lv9uf
@sahilKhan-lv9uf 3 года назад
Sar maei plating ka kam janta hun aap mujhe reply karo
@mdi786
@mdi786 3 года назад
@@sahilKhan-lv9uf mujhe plating ke liye admi chahiye apka number ya email address do
@sachinayre1788
@sachinayre1788 3 года назад
RECTIFIER purana style ka hai Naya igbt lagao
@rudrakshaaikar863
@rudrakshaaikar863 2 года назад
How make nickel plating dull
@sreenathkm9214
@sreenathkm9214 4 месяца назад
Without any safety respirator😅 Good luck
@lalbahadur142
@lalbahadur142 3 года назад
Load dalne ke 10mints bad nikalte samy current ku lgta hai plz my help
@obaidalam1581
@obaidalam1581 Год назад
Yes sir
@ronaldkarimi3302
@ronaldkarimi3302 3 года назад
I'd like to have a set up like this in Kenya . please share contact details.
@BluePlanetDesignStudio
@BluePlanetDesignStudio 3 года назад
+91 9979742116 Mr. Mit Gadhiya
@user-ks8gc1uq1q
@user-ks8gc1uq1q 3 года назад
Ye kaha pe karke milata hai.... Mumbai mai
@BluePlanetDesignStudio
@BluePlanetDesignStudio 3 года назад
Geet Gadhia : +91 98986 22616
@sarfarazmullamiraj7219
@sarfarazmullamiraj7219 3 года назад
Abs plastic ko plating karna hai agar sahi plating hone par bulk order may banana hai pls apna address & contact no chahiye
@BluePlanetDesignStudio
@BluePlanetDesignStudio 3 года назад
Geet Gadhia : +91 98986 22616
@rutvikseladiya
@rutvikseladiya 2 года назад
@Sarfaraz Mulla Miraj Aapka contact detail bhejiye email or no
@josesamuel136
@josesamuel136 Год назад
V danger chemical crome
@saveenvironment3997
@saveenvironment3997 3 года назад
Hello...sir...i am student BPKG iti CHAUKAGHAT in Varanasi..my trade is Electroplating...i have no job....my passing results 2017 to 2019...
@BluePlanetDesignStudio
@BluePlanetDesignStudio 3 года назад
Geet Gadhia : +91 98986 22616
@nkedesmond
@nkedesmond 3 года назад
dear sir, i am interested to set up a line in Malaysia, can you help us?
@sunilgadhia2458
@sunilgadhia2458 3 года назад
Yes...we can
@ronaldkarimi3302
@ronaldkarimi3302 3 года назад
@@sunilgadhia2458 please share contact details
@pranavanvekar4925
@pranavanvekar4925 3 года назад
Were can I buy those chemicals
@sunilgadhia2458
@sunilgadhia2458 3 года назад
Where are you from?
@eko653
@eko653 3 года назад
@@sunilgadhia2458 how much money chrome solution?
@NirmalKS123
@NirmalKS123 3 года назад
How much investment needed?
@thomasp.3842
@thomasp.3842 3 года назад
5
@BluePlanetDesignStudio
@BluePlanetDesignStudio 3 года назад
Geet Gadhia : +91 98986 22616
@ranggawijaya7572
@ranggawijaya7572 3 года назад
Lokasi dimno
@user-xs4is7jx5h
@user-xs4is7jx5h 4 месяца назад
منكن ترجمه بالعربي
@s.sankrasubbus.senthilkuma9362
@s.sankrasubbus.senthilkuma9362 3 года назад
தமிழில் பேசி விழக்கவும்
@Santoshchaudhary-iz2lp
@Santoshchaudhary-iz2lp 3 года назад
Establishe krne m ktna paisa lg jayega
@BluePlanetDesignStudio
@BluePlanetDesignStudio 3 года назад
Share Your contact details
@harshadshevale7222
@harshadshevale7222 3 года назад
Maze tr aprentes zale ahe
@alphaengineeringworks7302
@alphaengineeringworks7302 3 года назад
@@BluePlanetDesignStudio 8857888377
@BluePlanetDesignStudio
@BluePlanetDesignStudio 3 года назад
Geet Gadhia : +91 98986 22616
@maazali4283
@maazali4283 3 года назад
Teir
@asifshaikh5557
@asifshaikh5557 Год назад
Sir Mera bhi sem kaam hai ahemdabad mai
@user-co4rs7ob1t
@user-co4rs7ob1t 2 года назад
Вредная работа...пары кислот...
Далее
PH Tool's Nickel Plating Process
4:13
Просмотров 62 тыс.
would you eat this? #shorts
00:23
Просмотров 1,4 млн
Викторина от МАМЫ 🆘 | WICSUR #shorts
00:58
Аминка ❤️
00:16
Просмотров 595 тыс.
DIY Chrome Kit
3:14
Просмотров 4,5 млн
Coventya Plating on Plastics (POP) process
4:36
Просмотров 119 тыс.
Высокий Питер😂😄
0:52
Просмотров 1,1 млн