In this video I show you how to do a DIY home project to create stunning coloured anodising effects on titanium. All you need is distilled water baking powder and 9v batteries
------------------------------------------------------------------------------------------------------
Connect with me:
🔆 TikTok / themanwiththehat
🔆 www..themanwiththehat.co.uk
----------------------------------------------------------------
©️ Copyright 2023 All Rights Reserved

Развлечения

Опубликовано:

 

15 мар 2022

Поделиться:

Ссылка:

Скачать:

Готовим ссылку...

Добавить в:

Мой плейлист
Посмотреть позже
Комментарии : 284   
@williampatten2934
@williampatten2934 Год назад
As electrolytic rust stripping, this may work (though these batteries couldn’t provide the needed current) but especially when the new ‘colour’ appears to have formed above the liquid level as well “and” you can use any metal as a cathode…..this is a year around April Fools joke that sadly, some gullible folk may not see! These ‘simple way to do complex / impossible stuff’ are more unkind than funny. So for me it’s back to making my free electricity machine out of a computer fan
@vitabricksnailslime8273
@vitabricksnailslime8273 Год назад
My anti-vaxxing, 5G fearing, moon landing hoax proponent, Tesla worshipping, virtue signalling vegan, but so far free energy deprived (because of the conspiracy you know) son, sent me a good one. Something he really thinks is the bees knees. It's an electricity generator that you just throw in a river. It looked somewhat like the rotor of a push mower. I have to admit that it was shiny and had really good bearings. The fact that it wasn't connected to any sort of generator (or anything in fact) didn't seem to matter to the hordes of enthusiastic would be investors. After all, the guy looked like a really trendy counter-culturist. And he delivered his spiel in a room full of powerful electrical equipment. The real deal.
@garicrewsen1128
@garicrewsen1128 Год назад
Wait, so this is B.S.
@juggnautbitch
@juggnautbitch 5 месяцев назад
@@garicrewsen1128 No, i've seen people anodize titanium wheels bolt this way.
@marktucker208
@marktucker208 Год назад
Really clever, great job.
@stevesls007
@stevesls007 Год назад
Brilliant! Thank you very much!!
@ftswarbill
@ftswarbill Год назад
*Wow, Great video. Thank you!* 😃👍
@Slaktrax
@Slaktrax Год назад
Great idea! Thank youi 🙂 👍
@korbendallas9722
@korbendallas9722 Год назад
Great demo, but one piece of info that was incorrect is that once you anodize Ti, it’s there forever. You can remove ano by using something like Whink rust stain remover, and then you can start the process all over.
@andrewd5135
@andrewd5135 Год назад
could you use vinegar?
@MMPCTV
@MMPCTV Год назад
In the next video, the guy changes from one color to the next, just as stated in this video. ru-vid.com/video/%D0%B2%D0%B8%D0%B4%D0%B5%D0%BE-9Eut-Bu4Mpw.html
@GRBtutorials
@GRBtutorials Год назад
Be careful with it, though, it’s 1-2.5% hydrofluoric acid. That stuff has a reputation.
@krypticghxstgaming
@krypticghxstgaming 7 месяцев назад
@@GRBtutorials what does this mean? what does that do?
@HighlanderNorth1
@HighlanderNorth1 Год назад
☑️ Great video, I never realized it could be accomplished using such rudimentary items. I want to try this with niobium, but I've somehow misplaced the solid 10mm thick x 125mm long chunk of pure niobium round bar I bought as part of my element collection 18 years ago. Maybe it would be better to use a smaller, thinner piece for this purpose. I assume the thickness and overall mass of the substrate will play a role in how rapidly it'll anodize?
@TheManWithTheHat
@TheManWithTheHat Год назад
You can do it!
@melissae1116
@melissae1116 Год назад
Very nice, really cool.
@normanmastrian
@normanmastrian Год назад
Wow that was easy!
@YorkshiremanInDorset
@YorkshiremanInDorset 2 года назад
So many things I need to have a go at 😀 Thanks for sharing 👍💛
@TheManWithTheHat
@TheManWithTheHat 2 года назад
What you going to do?
@YorkshiremanInDorset
@YorkshiremanInDorset 2 года назад
@@TheManWithTheHat I’ve a few camping utensils which often get mixed up and “borrowed” by other people. If I colour them I’ll instantly know they’re mine 🙂 Will the same method work on aluminium alloys too? I’ll do some experiments 👍
@neenagalante1211
@neenagalante1211 2 года назад
Wow! So cool! Thanks for sharing!🙂🤗
@SandrasSpicySpanishSalami
@SandrasSpicySpanishSalami 8 месяцев назад
Fascinating! ❤
@sarahheetz5259
@sarahheetz5259 Год назад
Thank you so much for this video!!! I will be trying this tomorrow😊
@TheManWithTheHat
@TheManWithTheHat Год назад
Hope you like it!
@teddysimavari2612
@teddysimavari2612 Год назад
Brilliant video, I’ll have a go at this when I get time on some bicycle parts. I always though that anodising was a bit too complicated. Bit of a silly question but could you get black anodised using this method? Or is the best colour achievable just a really really dark brown? Also another silly question, there is no green. Is it possible to mix 2 colours to get one colour? Anyway, thanks again for sharing!
@pupyfan69
@pupyfan69 5 месяцев назад
if the parts are made of steel, bluing is a very simple process that would turn them black
@tmo314
@tmo314 Год назад
You’re a very interesting person! I had never heard of this
@slambk
@slambk 6 месяцев назад
Thanks very much
@stevenpillay5688
@stevenpillay5688 Год назад
Is it possible to do this process to fine silver or sterling.
@Biokemist-o3k
@Biokemist-o3k Год назад
New subscriber here. Fantastic!! Thank you so much.
@TheManWithTheHat
@TheManWithTheHat Год назад
Thanks for subbing!
@Biokemist-o3k
@Biokemist-o3k Год назад
@@TheManWithTheHat Absolutely. I am a chemical engineer however I never really looked into anodizing.
@stevejones9435
@stevejones9435 Год назад
What kind of power drain on the batteries will it cause? Are you able to use the same batteries for numerous applications? Thx for the video.
@thomasheisler
@thomasheisler Год назад
nice, no messing with acids and dyes
@dismayer666
@dismayer666 4 месяца назад
as well as not getting any result
@maderightamerica3216
@maderightamerica3216 Год назад
hmmm 🤔Maybe I can practice this method of anodizing and start making products to sell. The man in the hat is a really smart man for knowing the benefits of sharing knowledge. I think my future wife (a.k.a. boss) will like seeing this. hmmm🤔 Maybe not cuz she will make me do all the work while she goes shopping at the mall. 😂
@TheManWithTheHat
@TheManWithTheHat Год назад
🤪🤪🤪🤪🤪🤪🤪
@killzoldek6147
@killzoldek6147 10 месяцев назад
Thanks uncle
@ThePeterDislikeShow
@ThePeterDislikeShow Год назад
Can zinc be anodized? I'm reading tri-sodium phosphate might be used as the solution?
@Zubado1
@Zubado1 Год назад
Can these be done to cheap potash metals and aluminum?
@ErikOdinsvej
@ErikOdinsvej Год назад
after treatment, do it then not rost ?
@jcadona
@jcadona Год назад
Congratulation. Can you give more details of the paint used? Thanks
@garicrewsen1128
@garicrewsen1128 Год назад
What great hobby idea with zero learning curve! Thanks heaps for providing the voltage/color chart, BTW. IDK if you peruse your older video comments, but I've got a question: Does time in the solution make a difference in the saturation of the color or is it as pronounced as it's going to be in the first seconds of submersion? TIA. Cheers!
@TheManWithTheHat
@TheManWithTheHat Год назад
The colour change is immediate and immersed longer won’t do anything. Thanks for your comment
@FunnyFungusMonkey1928
@FunnyFungusMonkey1928 Год назад
I found found my new science fair project cuz it’s literally due in a week
@tomb816
@tomb816 Год назад
At 1:20 you say that you can't go back and the anodizing is there forever. this is untrue. It's actually very simple to reverse the color change (anodizing). Buy some Whink Rust Stain Remover (Hydroflouric Acid) and dip the part into it. It'll remove the anodizing, almost immediately. Rinse off the part in distilled water and your all set to try again.
@TheManWithTheHat
@TheManWithTheHat Год назад
Yes that’s true.
@SevenDeMagnus
@SevenDeMagnus Год назад
So cool.
@TheManWithTheHat
@TheManWithTheHat Год назад
Thank you pal
@JimBlair
@JimBlair Год назад
I believe most people identify anodising as an aluminum process, and the video is referring to a process on titanium…I find my titanium takes on a beautiful dark purple blue hue if it's sitting in the sulfuric acid for a few hours, during an anodising run...I'm not sure getting any other colours on titanium is possible?
@arasheqajar
@arasheqajar Год назад
This
@johnh8615
@johnh8615 Год назад
Yep it’s like when you weld titanium and you have these beautiful colours. You don’t get these on other metals so much.
@bermchasin
@bermchasin Год назад
whats the easiest way to do aluminum?
@williamemerson1799
@williamemerson1799 Год назад
@@bermchasin ru-vid.com/video/%D0%B2%D0%B8%D0%B4%D0%B5%D0%BE-P8oesBi7_II.html Don't know if it's what you call easy.
@mikealext
@mikealext Год назад
Its called heat tint. the different colors are different temperatures being reached.
@fredericksaxton3991
@fredericksaxton3991 Год назад
I assume that clean fresh rainwater is just as good as distilled water?
@Squidbush8563
@Squidbush8563 Год назад
So, I assume if you use a variable power supply you could put the object in at the lowest voltage and as you slowly pull it out of the water, turn the voltage up and get gradual rainbow coloring.
@TheManWithTheHat
@TheManWithTheHat Год назад
Yes, but it’s difficult finding a power supply which will go that high in voltage
@Squidbush8563
@Squidbush8563 Год назад
@@TheManWithTheHat Most will only go about 12 volts, unless you get a good bench power supply that can do 120V. cost around $80 - $100 but it's a lot safer than snapping batteries together. (Plus you can also use it for anodizing Aluminum)
@tomclanys
@tomclanys Год назад
@@TheManWithTheHat cheap bench supplies go to 30V, you can use a dual channel one in series for 60V, or use a variac with a rectifier and a resistor, or other current limiter.
@donm1547
@donm1547 Год назад
9 volt batteries connected in series can quickly sum to a lethal voltage, above 36 volts is about the threshold, I would wear dielectric gloves as one precaution.
@MOTO_DOSE
@MOTO_DOSE Год назад
@@donm1547 amperage kills not relatively low voltage such as 36v. As a mechanic I've been hit with 10,000v several times by ignition coils. Voltage doesn't kill. Amperage kills.
@rogerdempsey7227
@rogerdempsey7227 2 года назад
Great information Stephen 👍
@chaosopher23
@chaosopher23 Год назад
Cool! I have a power supply that can do up to about 600 volts... but another that can variable up to 120 volts. Those transistor batteries can get a bit expensive, and my Li rechargeable only put out 8 volts.
@user-xf7rr2pu2h
@user-xf7rr2pu2h 11 месяцев назад
will this work with tungsten? as im planning to do it with darts.
@oldrobone
@oldrobone 2 года назад
can you use deionized water instead of distilled water
@Jesus_Wojak
@Jesus_Wojak Год назад
I think the mayne problem would be the trace minerals like chlorine. You dont want chlorine gas in your house.
@alexisferrer6859
@alexisferrer6859 Год назад
How many batteries for gold?
@martynj-c4965
@martynj-c4965 Год назад
How can I get bolts and washers etc in bronze please? Thank you
@Umski
@Umski Год назад
Watch out utensil drawer - have distilled water, will anodise 😁
@ph11p3540
@ph11p3540 Год назад
I would be nervous of having 9v batteries series together like that. Don't their terminals get really hot when they directly touch each other like that?
@WAINTDEIR
@WAINTDEIR Год назад
Connecting them in series just increases the Voltage. As long as you dont short the poles (or lick the outer most poles 😅) nothing should happen... but there is still a Voltage of 45V when theese 5x 9V batteries add up...
@TheManWithTheHat
@TheManWithTheHat Год назад
Thank you for explaining that to Philip I really appreciate that
@mikedillard835
@mikedillard835 Год назад
...luv it !....with my luck I'll blow up the house...
@TheManWithTheHat
@TheManWithTheHat Год назад
😂😂😂😂😂
@paddingtonsnare987
@paddingtonsnare987 11 месяцев назад
I've got a chromoly frame.. will it anodise?! I'd need a pretty giant container though🤔
@girliedog
@girliedog Год назад
Does this work the same for aluminum?
@TheBaconWizard
@TheBaconWizard Год назад
Nope, titanium only.
@breannestahlman5953
@breannestahlman5953 Год назад
Thanks for your video, that is new to me. Will this protect from rust? Can it be done with a charger, like a phone charger or a transformer, like 220v to 3, 6, 9,12 v, etc . . .? Does it absoluyely needs those 9v batteries or any could do it, as long as you provide the level of power?
@TheManWithTheHat
@TheManWithTheHat Год назад
It can be done with a variable voltage rectifier
@kaykaydesign6520
@kaykaydesign6520 Год назад
Is this process works with regular nuts and bolts? I want to anodize my scooter engine bolts...how to do it to make it turn purple...
@TheManWithTheHat
@TheManWithTheHat Год назад
Only on Titanium bolts
@RcNerd
@RcNerd Месяц назад
Try a stepper power box adjust the v and you can do loads
@smallick653
@smallick653 Год назад
Can we anodized aluminium pannel in the same process?
@TheManWithTheHat
@TheManWithTheHat Год назад
Not at all because you need a dye for aluminium
@chrischoir3594
@chrischoir3594 9 месяцев назад
Does this work with 6061 T6?
@jamesbaker7112
@jamesbaker7112 Год назад
I was startled to learn this. Subscribed.
@TheManWithTheHat
@TheManWithTheHat Год назад
Thank you. Are you going to try it
@jamesbaker7112
@jamesbaker7112 Год назад
@@TheManWithTheHat I kinda have to.
@charlespeagler8010
@charlespeagler8010 Год назад
um, if i remember correctly using stainless as an anode the electrolysis process gives off a chlorine gas, which is poisonous as hell. tin, aluminum foil, steal cans cut into strips can all be used.. granted ive not looked into titanium process, but aluminum is done will low voltages 5-12 v low 2-4 amp also fabric dyes get used in process. seen it done with cpu power supplies and low amp batter chargers.
@MrSunrise-
@MrSunrise- Год назад
There is no chlorine in the system - he's using baking soda and distilled water.
@Squidbush8563
@Squidbush8563 Год назад
@@MrSunrise- yea. at the very most it will produce C02
@glawson1139
@glawson1139 Год назад
@@MrSunrise- That;s baking POWDER -not soda- 2 different things..
@wes.killed.it.5511
@wes.killed.it.5511 4 дня назад
@@glawson1139 Baking soda is actually the correct mixture to be added to the water. The videos creator did say baking power but this is incorrect, since baking soda is the correct ingredient to neutralize the solution. Borax can also be used in place of baking soda; however, baking powder will not suffice as a neutralizer. I have about 25 hours of titanium anodizing experience and I will say the baking soda has given better results than the borax/distilled water solution.
@raketoped663
@raketoped663 Год назад
This is pretty cool, thank you. I will definitely try this
@raymondojones3830
@raymondojones3830 10 месяцев назад
Great work, can you use a car battery?
@Durplepurple94572
@Durplepurple94572 Год назад
Can this method be used to anodize Aluminum to give it more scratch and wear resistance?
@TheManWithTheHat
@TheManWithTheHat Год назад
No. It does say that in the video.
@easternbushytail
@easternbushytail 5 месяцев назад
I did this to a piece of titanium and after it was done to the color I desired, it turned a dark gray color after I touched it. What did I do wrong? Thanks.
@tonybirdwell2624
@tonybirdwell2624 2 года назад
Thanks! I need to give this a go.
@TheManWithTheHat
@TheManWithTheHat 2 года назад
Amazing what you can do Tony
@tonybirdwell2624
@tonybirdwell2624 2 года назад
@@TheManWithTheHat I have a lot of keys ,to go through when I need to get inside of the different buildings.
@spanish_boiya.g9920
@spanish_boiya.g9920 2 года назад
@@TheManWithTheHat Hi sorry, I know you used tantanium, would it work with stainless steel the best?, I haven't seen a video to confirm it
@fosterck13
@fosterck13 18 дней назад
What does technique work for gemstone beads
@asensibleyoungman2978
@asensibleyoungman2978 7 месяцев назад
How come you don't get a shock from the water and the electricity?
@aixpert291
@aixpert291 Год назад
Holy crap!
@Marinesniprx
@Marinesniprx 4 месяца назад
Does it have to be titanium?
@robiruzic
@robiruzic Год назад
this is on titanium what about on other metal parts??? doesn't seem to work
@SevenDeMagnus
@SevenDeMagnus Год назад
New subscriber here.
@TheManWithTheHat
@TheManWithTheHat Год назад
Thank you so very much
@JohnDavis-yz9nq
@JohnDavis-yz9nq Год назад
Would have liked to see the results.
@TheManWithTheHat
@TheManWithTheHat Год назад
Then why did you watch the entire video?
@andreashenriksen1485
@andreashenriksen1485 Год назад
@@TheManWithTheHat damn my mans. Be happy that he did..
@CertsUAsPilot
@CertsUAsPilot Год назад
Does this method only work on titanium?
@TheManWithTheHat
@TheManWithTheHat Год назад
It tells you in the video
@LOLLO2WIN
@LOLLO2WIN Год назад
It isn't working can you make a more in depth tutorial for how to troubleshoot
@garicrewsen1128
@garicrewsen1128 Год назад
scroll up to the comment that says this is B.S. Enjoy!
@Havanacuba1985
@Havanacuba1985 Год назад
I couldn’t see the color ?
@shekerrichdell5825
@shekerrichdell5825 Год назад
it works in stainless ???
@jordanm6836
@jordanm6836 Год назад
It can be but if you wanted to prevent the color from fading you have to seal it.
@martinweizenacker7129
@martinweizenacker7129 Год назад
So would this work with plain, standard run-of-the-mill galvanized screws, nuts and so forth?
@TheManWithTheHat
@TheManWithTheHat Год назад
You didn’t watch the full video did you?
@martinweizenacker7129
@martinweizenacker7129 Год назад
@@TheManWithTheHat I did. You say get some screws from the local hardware store. But I always ever heard of this working with Aluminium, so it is unclear to me if you really mean regular galvanized screws.
@justinw1765
@justinw1765 Год назад
@@martinweizenacker7129 The video only addresses using this method on titanium.
@garicrewsen1128
@garicrewsen1128 Год назад
@@justinw1765 Yet he mentions steel, the first piece of metal to go into a jar in this video, and aluminum foil giving specific instructions not to let the leads touch right after talking about aluminum foil. Confusing. Why mention the other metals, let alone show a steel strip being place in a jar about to be anodized? Question is rhetorical.
@dekutree64
@dekutree64 6 месяцев назад
@@garicrewsen1128 The other metal is just to make electrical contact between the battery and water to complete the circuit.
@relaxingpill7525
@relaxingpill7525 Год назад
What type of metal can you anodized? Stainless steel? Aluminum?
@TheManWithTheHat
@TheManWithTheHat Год назад
Doh. I told you I’m the video
@drewrinker2071
@drewrinker2071 Год назад
I believe he said titanium. Aluminum is more complex and involves harsher chemicals
@sanderaits
@sanderaits Год назад
@@TheManWithTheHat You mentioned titanium like 2 times in the video and only in the end and the mentions are so casual like you randomly picked a titanium chopstick to show this off. You even say to go the hardware store and pick some screws and try on that, you never say it ONLY works on Ti.
@runman1
@runman1 Год назад
@@sanderaits EXACT
@jesusblessthesecommentsamen
@jesusblessthesecommentsamen 2 месяца назад
How many batteries for black ?
@pretotzkie4031
@pretotzkie4031 Год назад
how many batteries for black?...
@TheManWithTheHat
@TheManWithTheHat Год назад
300
@Chris.Rhodes
@Chris.Rhodes Год назад
So can you do this with stainles steel?
@TheManWithTheHat
@TheManWithTheHat Год назад
No
@Chris.Rhodes
@Chris.Rhodes Год назад
@@TheManWithTheHat damn. ok thanks
@j.csamson1512
@j.csamson1512 10 месяцев назад
This technique works any metals????
@TheManWithTheHat
@TheManWithTheHat 10 месяцев назад
It told you in the video.
@adullahtarawneh8639
@adullahtarawneh8639 Год назад
Will this work on silver?
@TheManWithTheHat
@TheManWithTheHat Год назад
Watch this video properly have you?
@mohadam1182
@mohadam1182 Год назад
Can you do it with filtered water?
@TheManWithTheHat
@TheManWithTheHat Год назад
Try it and see.
@WauanSuargo
@WauanSuargo 7 месяцев назад
Is it possible to use something other than titanium? for example like iron please reply my lord 🙏
@dekutree64
@dekutree64 6 месяцев назад
Not with electricity, but steel (including stainless) will grow a colorful oxide film when heated. Difficult to get the exact color you want when heating with a flame, but it's fun and easy to get semi-random colors.
@WauanSuargo
@WauanSuargo 5 месяцев назад
@@dekutree64 thank's
@soumyajitmohanta26
@soumyajitmohanta26 7 месяцев назад
How can I get rainbow colour
@your_uncle_barry_6700
@your_uncle_barry_6700 Год назад
Does this work on any metal or just titanium?
@TheManWithTheHat
@TheManWithTheHat Год назад
So many people ask me that which means they never watch the full video.
@your_uncle_barry_6700
@your_uncle_barry_6700 Год назад
@The Man With The Hat now there's no need to make assumptions I most definitely watched the full video. I heard you saying you used marine steel I think it was but I didn't think that was the piece that got anodised. I've had an awful day everything has gone wrong so I've been in a constant state of stress so I guess I wasn't paying enough attention. Or if so many people have asked you that maybe it just wasn't made clear enough. I'll watch the video again but thankyou for your reply
@runman1
@runman1 Год назад
Sorry but I wat the full video many times.. you mention marine steel for negative and titanium chupstick OR screws or someting at your hardware store.... it's very vague on the type of metal to use
@your_uncle_barry_6700
@your_uncle_barry_6700 Год назад
@runman1 yes I heard that. go get some screws or something but he uses titanium chopsticks. So are all screws titanium? Or do I need to find titanium screws? Or did he mean any metal? because that's what it sounds like. Glad it's not just me. And when you click the comments section one of the two guidelines is "questions welcome"..... well clearly that depends on the question. I'll go watch someone elses video who will tell me straight what metals I can use instead of dancing around the question. "So many people ask me that", yes for some reason I am not suprised
@camerongray9844
@camerongray9844 Год назад
Where can I get a copy of that chart?
@TheManWithTheHat
@TheManWithTheHat Год назад
Search the Internet
@garicrewsen1128
@garicrewsen1128 Год назад
SS or screen snip at the appropriate frames.🎥🎞📽🎬
@smoklares9791
@smoklares9791 5 месяцев назад
Does this produce no poisonous gas? With stainless steel?
@TheManWithTheHat
@TheManWithTheHat 5 месяцев назад
Nope
@josephybarra3555
@josephybarra3555 Год назад
Can you anodize aluminum?
@TheManWithTheHat
@TheManWithTheHat Год назад
No
@DavidWilliams-bu8xt
@DavidWilliams-bu8xt Год назад
Tell that to my job at lintec lol that’s all I do is anodize aluminum😅
@justinw1765
@justinw1765 Год назад
@@DavidWilliams-bu8xt Not through this exact method. Obviously Al can be anodized, speaking generally.
@Freedm762
@Freedm762 Год назад
Question: can you do this with stainless steel that's already colored?
@TheManWithTheHat
@TheManWithTheHat Год назад
You can’t do stainless at all.
@Freedm762
@Freedm762 Год назад
@@TheManWithTheHat i see
@garicrewsen1128
@garicrewsen1128 Год назад
@А I mistook the same thing, but the steel and aluminum are the anode in the process, which is particularly unclear in this video. Confusing and frustrating.
@immanueldorai
@immanueldorai Год назад
DC current is more dangerous and fatal than AC current. Secondly the the route the flow of current takes through the body is also very important in deciding the fatality. Wear proper gloves while handling electricity.
@nathandevine552
@nathandevine552 Год назад
I disagree ac will grab you and you can't let go ask anyone who has gotten stuck to a old ac welding machine DC you can let go of
@immanueldorai
@immanueldorai Год назад
@@nathandevine552 Sorry brother. It is the other way. AC breaks 50 or 60 times a second, but DC does not. DC will burn through your skin like welding arc. I have worked on Radar systems for 26 years where we work with DC voltage of 6 to 12 Kva and 2 to 12 amps. I have seen our heavy gauge screw driver literally melting when accidentally shorted within seconds. So please remember DC current is fatal compared to AC. Ofcourse even above 100ma can harm you.
@nathandevine552
@nathandevine552 Год назад
@@immanueldorai at those voltages and currents you worked with in radar either will be fatal and have explosive results if shorted. at 120~240 you can get stuck to AC DC will just shock you now either can kill you but there is so many variables like as you said the path it takes threw your body......I've been zapped by DC welders not that big a deal I got stuck to a AC machine and would be dead if my friend hadn't had the sence to switch it off
@immanueldorai
@immanueldorai Год назад
@@nathandevine552 everyone has his own experiences. In India we use 230 volt 50 hz and have experience of coming in contact with domestic electric wiring and points. Not much harm done till date. Welding is all together is a different story. Low DC voltage but very high current upto and above 200 amps. Just sharing my experience as a technician and instructor in Airforce since 1975. Your experiences may be different.
@jeffjeff8562
@jeffjeff8562 Год назад
Why would you stop the camera at 1:44 and resume it if this is so quick and simple?
@TheManWithTheHat
@TheManWithTheHat Год назад
Because I can.
@guesswho6761
@guesswho6761 Год назад
Im just wondering, what make you bought Titanium chopsticks
@mjremy2605
@mjremy2605 Год назад
MADE YOU BUY, not MAKE YOU BOUGHT. Use correct grammar and tense please.
@guesswho6761
@guesswho6761 Год назад
@@mjremy2605 ok....what do you expect? I got c on final English test, i didnt pay attention in class and its my 2nd language Jezz, grammar polices are everywhere
@TheManWithTheHat
@TheManWithTheHat Год назад
Forget him he’s an arsehole
@schafer240
@schafer240 Год назад
@@mjremy2605 Y U SO Mad?
@ElegiesAus
@ElegiesAus Год назад
Will this process work with mild steel? I’m an Engineering teacher and my students made a quick bottle opener project to learn basic hand skills. Unfortunately, part of the bottle opener is made from mild steel which wants to rust.
@TheManWithTheHat
@TheManWithTheHat Год назад
No
@jordanm6836
@jordanm6836 Год назад
Only Aluminum and Titanium can be anodized. Aluminum cannot be done as easily as Titanium. Aluminum needs some additional chemicals and dye. Titanium can also be heat anodized using a torch. In terms of doing something with mild steel, you can do a black oxide coating I've you're trying to do something cooler than just spray paint. Check it out. ru-vid.com/video/%D0%B2%D0%B8%D0%B4%D0%B5%D0%BE-TFfJwNvK1iY.html
@oldrobone
@oldrobone Год назад
Try looking up nickel plating I believe that will stop the rust problem
@minimogmulah
@minimogmulah Год назад
It's been a long time since I was at school, but I remember making a bottle opener, we were made to sand it down to remove all the oils from our hands, then when it was clean, dipped it in a quenching oil and burnt it off to leave a nice oil effect. Others used coloured glass tubes to make patterns once they were burn down
@drewrinker2071
@drewrinker2071 Год назад
Teach them how to blue the mild steel,that's a fairly simple process, heat it up to a certain temperature and dip it in oil. You could cheat and buy super blue also but that's not really going to teach them anything
@edwardfletcher7790
@edwardfletcher7790 Год назад
Might be easier long term to use a cheap variable power supply than waste dozens of 9v batteries....
@TheManWithTheHat
@TheManWithTheHat Год назад
I have two power supplies but that defeats the objective of showing ppl how to do it with batteries.
@rodmills4071
@rodmills4071 Год назад
@@TheManWithTheHat some people just don't get it, do they.🤔😂😎🇦🇺👌
@kingdavid99887766554
@kingdavid99887766554 Год назад
You mean to tell me that anodizing only uses electricity?
@TheManWithTheHat
@TheManWithTheHat Год назад
Voltage
@Secret_Squirrel_Scottishgamer
how to turn your peen green in 3 seconds... "OUCH" lmao
@wrinkle1784
@wrinkle1784 2 года назад
How do i anodize it black?
@TheManWithTheHat
@TheManWithTheHat 2 года назад
Good question. I have no idea.
@sarachitamang6840
@sarachitamang6840 2 года назад
Sir what does chmical mix ?sir please
@keithhansen3963
@keithhansen3963 Год назад
Thank you for the video. Is this specific to Titanium or does it work for Aluminum and regular steels?
@TheManWithTheHat
@TheManWithTheHat Год назад
Only titanium
@garicrewsen1128
@garicrewsen1128 Год назад
@@TheManWithTheHat You stated it also works with steel and aluminum foil.
@EL34XYZ
@EL34XYZ Год назад
The vertical camera format is annoying. Turn the camera horizontally to film for RU-vid.
@TheManWithTheHat
@TheManWithTheHat Год назад
Piss off
@geoffgeoff143
@geoffgeoff143 Год назад
You are dealing with potentially lethal voltages.
@TheManWithTheHat
@TheManWithTheHat Год назад
Rubbish? There’s only 6 batteries. Explain why this is lethal
@petanipemulaporangatlkapul4481
@petanipemulaporangatlkapul4481 2 года назад
Can we do at stainless steel material ?
@TheManWithTheHat
@TheManWithTheHat 2 года назад
No
@stainlessca4837
@stainlessca4837 Год назад
@@TheManWithTheHat curious because you use stainless steel in your video? I'm not presuming you know, but I'd like to colorize a 20ga. stainless sheet with #4 (brush) finish... any ideas? I believe heating works but afraid it'll warp the panel (about 30" square) also
@garicrewsen1128
@garicrewsen1128 Год назад
@@stainlessca4837 I made the same mistake. The stainless he showed and the aluminum foil he mentions during those frames are the anodes in the process. He doesn't cover that and that's why so many querying about the two metals.
@roonimac
@roonimac Год назад
So many people are saying it doesn’t work.
@TheManWithTheHat
@TheManWithTheHat Год назад
I just did it live on camera. This who cannot make it work probably didn’t even go to school.
@garicrewsen1128
@garicrewsen1128 Год назад
@@TheManWithTheHat Or they had crappy teachers.
@joluju2375
@joluju2375 Год назад
Instead of steel I tried with a gold fish, and the result was disappointing.
@TheManWithTheHat
@TheManWithTheHat Год назад
You got a lovely orange colour tho
@mrgeraldbrent
@mrgeraldbrent Год назад
Be very very careful running too many batteries in series. HVDC is no fuckin joke. There's a video on RU-vid of some guy that managed to get 900v out of a bunch of 9 volts chained together, and you could hear them arcing to eachother even with nothing connected.
@TheManWithTheHat
@TheManWithTheHat Год назад
Well, that’s 100 batteries. I’m only using six
@PatriotCoinRings
@PatriotCoinRings 11 месяцев назад
*"COUPLE OF QUESTIONS I'M SURE EVERYONE WOULD LOVE TO KNOW"* Everyone seems to have a different approach on their choice for electrolytes. I've been using fire (MAP and Propane annealing) for years but I'm trying to up my game... *1.* Being a jeweler, I do a ton of gold and precious metal plating so have all the equipment for professional full submersion anodizing but only now getting into it in an attempt to achieve smoother, more controlled coloration. While I know you said you use baking powder, another video said baking soda was much better and AI Chat seemed to agree asking which is better for anodizing. I've also been told vinegar is better, but stronger electrolytes like sulfuric acid or common salt (sodium chloride) are best. Do you have any thoughts on all this where you may have tried a few of these methods for comparison? *2.* Also, if not using the 9v battery run everyone seems to be recommending for power having a Lab Grade [LED High Precision Variable Adjustable 0-30V 0-5A DC Power Supply, what Votage and what Amperage do you recommend? *3.* Finally, should the Cathode be Iron like some have told me or stainless steel (which is what I'm very use to using for gold and precious metal plating)?
@TheManWithTheHat
@TheManWithTheHat 11 месяцев назад
The last thing first. The Cathro should always be marine grade stainless steel. The reason I use batteries in this demonstration is so that anybody can do a one off piece at virtually little cost whereas the professional kit would cost hundreds of pounds and therefore wouldn’t make such a good video For everyone in order to be inclusive. I have never tried anything other than baking powder, but I am willing to give it a go and post the results
@PatriotCoinRings
@PatriotCoinRings 10 месяцев назад
@@TheManWithTheHat Totally makes sense about why not to use Sulfuric acid but common household salt might be a good one for you to try. Don't get me wrong, I'm not critiquing what you are doing here as like I mentioned I'm a gold and precious metal plater, not an anodizer and only going off of what others have told me is best. Yesterday I did try a combination of salt and vinegar which I think I may have made far too strong but it literally melted my stainless steel making it look like it was just bleeding blue ink in the water and I was only using 3 volts @ 1.6 amps. I plan on trying your method this week but want to get some comparative results experimenting with different things as well..
@flowerpt
@flowerpt Год назад
I listened twice to be sure - typical misleading TikTok trash is what the block button was invented for. This will not work to anodize typical hardware store screws and he knows it.
Далее
Will it Black an Entire Aluminum Part?
21:19
Просмотров 1,2 млн
SIMPLE tech. Battery draws on metal
9:15
Просмотров 16 млн
Anodizing Titanium
10:59
Просмотров 117 тыс.
"Make It Pop!" DIY Titanium Anodization | How To Knife
6:51
Making TNT
20:40
Просмотров 1,4 млн
Four Steps to Flawless Wire Joints (How to Solder)
11:45
DIY Anodising Motorcycle Parts!
6:23
Просмотров 487 тыс.
Переиграл
0:20
Просмотров 1,1 млн