MET Basic Training: Brunauer - Emmett - Teller (BET) Surface Analysis
Materials & Energy Technologies Service Center
Conn Center for Renewable Energy Research
University of Louisville
M. Shahinur Rahaman, graduate student super user at Conn Center for Renewable Energy Research, shows how to set up and use the Brunauer - Emmett - Teller (BET) Surface Analysis in the University of Louisville's Materials & Energy Technologies Service Center.
0:12 Section 1: Preparing Samples for Degassing
1:38 Section 2: Degassing Samples
5:08 Section 3: Sample Loading in Analyzer
8:05 Section 4: Programming Values for Scans
15:40 Section 5: Report Files
16:46 Section 6: Process Assistance & Parameter Selection
18:00 Section 7: Shut Down Procedure
© 2020 University of Louisville
15 ноя 2020