Verify the quality of the MgO compaction inside heating elements
👉 www.csmmachine...
Heating elements exiting the roll reduction mill can have different lengths. This may be due to a defect in the MgO compaction that can be caused by a possible malfunction of the filling machine.
Since the compaction of the magnesium oxide (MgO) inside an heating element is a key feature for the subsequent production processes, it is necessary to verify the filling quality of heating elements and thus the status of the filling machine.
Necessary tools for the test: tubes, plastic plugs, MgO, tape, water and a balance.
***********
00:06 Preparation of sample tubes
01:03 MgO filling
01:48 Weighing
03:19 Calculation of the MgO density
***********