We were given a briefing on their JinChan Gold Dressing agent mixing and their pregnant solution pond by Khazaine's site manager. Gerak Darma's team is in the Khazaine Company gold processing plant on their compound in Sfariât, Tiris Zemmour Region, Mauritania. The site manager explained to us the mixing of the tailings/ore with lime before being spread in the VAT-leaching ponds, mixing the JinChan Gold dressing agent with water, pumping the leaching solution from the mixing pond to the VAT-leaching ponds, and collecting the pregnant solution in another pond after 12-14 days. The wind blew hard, and listening to the site manager talking was hard. We managed to get the ratio of the mixing for feed material (tailings/lime), leaching solution (water/JinChan), and leaching (leaching solution/tailings). We salute the site manager for trying his best to explain in English. He is only fluent in Arabic and French. The next briefing will be on the activated carbon tanks.