Simple tools work! the end result is all the proof required 👍👍👌👌💪💪💪 I really enjoy your videos sir. Cheers! By the way, I love the indexing head, well done.
For clean, polished and finished machining (on aluminum), use kerosene, not oil, and the tool must be made of high-speed steel. Congratulations. Para usinagem (em alumínio) limpa, polida e acabada, use querosene, não óleo, e a ferramenta deve ser feita de aço rápido. Parabéns.
Yet it used to be. I remember having lathe/ machining taught 1956-1959 and teacher did his own smelting// Local (Bayside, Trenton) had welding and machining shop until about 1995 when it was sold off. School now has over 1000 students!!!!
Exactly, tech college 1959-1963 taught this type of material handling, welding,smelting,casting, soldering, turning,smithing etc. Safety concerns put an end to it perhaps? I used to turn large asbestos pipe to fit resistance wire ,for variable resistors, no mask, no extractor....76 yrs old now,escaped any ill effects?
The aluminum has lots of holes in it due to impurity and gas. I found that if you make ingots from your scrap much of the impurity separates when you remelt them. Use of flux and degasser before skimming the slag works well. In addition poring thru a screen dam will leave you with very nice result without holes.
Or while your at it why not pony up 50k usd for a used live tooling cnc, another 10k in tooling, and a proper melt furnace, and better stock material? HE DOESNT HAVE IT.. and hes not gonna chop up what he does have when what he is doing works just fine. When you post a vid making what he does with what hes got then you will get respect.
In Britain, nothing like this is taught in schools. The health and safety nuts forbid it. We don't make things in our country, we just import it ( which explains our apauling trade gap) 😢
Pahat muka, pahat kiri mending pakai vidia aja bang, hss kalau untuk besi cor atau besi yang keras kurang kuat ( lebih kuat pahat vidia) Semua pahat bubut sudah ada videonya bang di playlist saya..