Hi Jason, I love your videos as I have just started electroforming and find you are the most informative!!! Question for you though...I noted in one of your videos with your copper tubing sets on either side of the tank that you mentioned 1 set was connected with a negative connection (same as cathode) and the other tubing was connected with positive. I was surprised as I thought both would have been connected +. Can you explain this? Thanks and keep the videos coming. Cheers, J
Mine come out of the bath covered in a grayish maroon silt. The copper plating Under it is light and seems to not plate scratches. Is that maroon silt normal? Also is there such a thing as too high of a voltage like 12v running at 1 amp?
I’m using vinegar because it’s safer but that’s at best a ph of 3. I’m doing this inside my house. Is adding a little bit of sulfuric acid from a car battery kit ok?
Hi, great vids, but If my solution goes bright red, then what do i do? A brand new copper plating solution also went bright red so how can i tell how to fix mine if they both look similar? Thanks again for the helpful information.Also when you put the drop of acid copper solution in the cabbage do you shake it in or just leave it? I have no idea sorry, and am new to all this. my copper solution lasted a good 8 months before i changed the copper then supplied it with and ever since it sucks. I heard we had to use phosphorus deoxidised copper is that true or preferred or i don't know because you don't seem to?