@imchris5000
@imchris5000 3 года назад
another way to add in copper is the little bits that end falling off and sinking to the bottom especially when your trying to blast out a tree top looking deal which I like using a shell chase as the base and if I dump amps in with where I want it to grow pointed at my anodes. it makes these crazy growths then ill crank the amps way down and let it slowly grow and rotate it from the anode so it wants to plate more than grow but I like the crazy coral shipwreck looking stuff especially after you get a little patina on it
@highvibemysticallifestyle
@highvibemysticallifestyle 5 лет назад
oops! I left my anode in for a few months while dealing with surgery and health issues. Gonna go clean it all up now!
@drewwhitaker315
@drewwhitaker315 5 лет назад
Nice talk, brother!
@sarahkoelbl368
@sarahkoelbl368 5 лет назад
Perhaps I'm barking up the wrong tree but what if you like the glittery finish? How do you make it happen on purpose?
@Kindnessmatters2
@Kindnessmatters2 5 лет назад
Thank you...: )
@sarahroy5320
@sarahroy5320 4 года назад
This is very helpful! For option A How long do you recommend leaving a piece in the bath at .34 amps per inch to balance your liquid?
@marlolyda8698
@marlolyda8698 3 года назад
These are such valuable question. I also want to know if you calculate the inch of anode with surface area too or just inch length into bath? Would be great to get some replies from Jason or other experts to my question and others
@cb175s
@cb175s 5 лет назад
I had a batch of rings turn out glittery and they look really cool. Lol It was my last batch with dirty tanks before clean up. I thought something got in the tanks or ? Over saturated sounds more logical. 👍
@Cloakfiend
@Cloakfiend 5 лет назад
I het the glitter deposit stuff all the time!!! Well anoying!
@awakenbeauty.boutique
@awakenbeauty.boutique 4 года назад
Would anyone know why the copper would not stick or hold in the mold 💯. And why it comes off when I file it. 😢
@FastNFishious
@FastNFishious 3 года назад
I believe your amps are to high for the square inch so it’s attaching super quick aka flake. If it’s organic material be sure it’s sealed prior to the bath.
Далее
Finishing Copper electroformed pieces
18:21
Просмотров 12 тыс.
СМОТРИМ YOUTUBE В МАЙНКРАФТЕ
00:34
Просмотров 1,4 млн
Random tips when producing Electroformed Goods 2021
28:04
PH balance your Copper Electroform Tank
9:24
Просмотров 10 тыс.
Protecting Stones when Electroforming
11:24
Просмотров 24 тыс.
Many Moving Magnets Melting Metal
20:21
Просмотров 2,9 млн
The Truth About SIM Card Cloning
13:04
Просмотров 1,1 млн
How To Identify An Unmarked or Blown IC Chip
32:31
Просмотров 43 тыс.
How Many ERRORS Can You Fit in a Video?!
20:40
Просмотров 2,7 млн
Советы на всё лето 4 @postworkllc
0:23