Ribbon Cables Gold and Silver Recovery using Cupellation method EXPERIMENT 

MetalScrapLab
Подписаться 1,6 тыс.
Просмотров 3,1 тыс.
50% 1

Experimenting with cupellation method to recover gold and silver from gold and silver plated ribbon cable connectors.
Table Top RapidFire Pro Metals Melting Furnace: amzn.to/3IDRtym
#12 Mabor Cupel 3-1/8" - Case 45: www.lmine.com/mabor-magnesia-...

Опубликовано:

 

8 авг 2024

Поделиться:

Ссылка:

Скачать:

Готовим ссылку...

Добавить в:

Мой плейлист
Посмотреть позже
Комментарии : 29   
@peteoneill5799
@peteoneill5799 4 месяца назад
Well done for giving it a go. Obviously not the most profitable endeavour but I commend your attempt
@andreabc1469
@andreabc1469 4 месяца назад
what a cool Grinder😍
@disgruntledgrunt241
@disgruntledgrunt241 4 месяца назад
The cost of electricity to do this must outweigh the value of the end product.
@prospectorpete
@prospectorpete 4 месяца назад
No it doesnt
@talavs-jekabsriekstins578
@talavs-jekabsriekstins578 4 месяца назад
+ the time and Bismuth
@wszechmocnieuzdolniony
@wszechmocnieuzdolniony 4 месяца назад
Witam witam i pozdrawiam serdecznie z Polski 🇵🇱👍👍👍
@kenpeters8257
@kenpeters8257 4 месяца назад
It would take buckets of that just to get enough to weigh. It is the fools Gold of E-waste.
@prospectorpete
@prospectorpete 4 месяца назад
Theres actually alot of gold in those
@NAFOARMY
@NAFOARMY 3 месяца назад
To all beginners (not this guy, he's smart and knows already) start with 2-3 grams of 10k gold scrap. Then you can see the process and get enough gold back to know you didn't fail. Most guys get 0.1 gold at the end orless because they do to little ewaste, and they dont see the 0.1gram and assume they failed when they really didnt. If you do enough to see the process start to end, youll learn a lot! This dude knew there wouldnt be much gold to see, he did it right (not my way though) and knew it was to little to expect much gold.
@guytelfer1353
@guytelfer1353 4 месяца назад
Good video, check the splatters in the oven
@frantiseklaluch6605
@frantiseklaluch6605 4 месяца назад
I also use bismuth, made own bone ash cupels, but was disaster a bit... 🙂 Under cupel I use terracota dish with magnesium oxide to avoid sticking. You did everything right, just not much gold and silver there...
@MetalScrapLab
@MetalScrapLab 4 месяца назад
Thanks, I still don't know where the dark liquid stuff came from when my first cupel with gold cracked and leaked because I only added bismuth and no flux.
@frantiseklaluch6605
@frantiseklaluch6605 4 месяца назад
@@MetalScrapLabHmmm... probably oxides, that were created in the ceramic dish, as liquid bismuth leaked, was oxidised in the dish, but liquid oxides had no way to be absorbed, so stayed as they were, as black liquid... For that case I have magnesium oxide powder under cupel, if things go south, MgO catches whatever...
@MetalScrapLab
@MetalScrapLab 4 месяца назад
Interesting. Thanks.
@freekingawwsome
@freekingawwsome 4 месяца назад
​@@frantiseklaluch6605 nice idea
@damienperry5758
@damienperry5758 4 месяца назад
From what I understand, you should turn your furnace down to like 1000’ with bismuth. It splatters your PM everywhere when you get it too hot
@maxcloutier5285
@maxcloutier5285 4 месяца назад
Humm, its gone a take time before we retire with this gold !
@guytelfer1353
@guytelfer1353 4 месяца назад
No black or dark nuggets? Maybe the plastics is on the gold( thought it was borax. You need a substantial amount of material to get a gram
@user-xd8bk7cx4n
@user-xd8bk7cx4n 4 месяца назад
I don't know if that was even worth the trouble.
@prospectorpete
@prospectorpete 4 месяца назад
If he did it in a different way its definately worth it
@FACTUALITY-1
@FACTUALITY-1 4 месяца назад
So, after expenses and paying taxes, how much do you make an hour? I'll bet it's not enough to pay the bills.
@2001pulsar
@2001pulsar 4 месяца назад
Bismuth is not as good as lead for cupelling. MBMM Jason found losses with bismuth compared to lead in the same process for both.
@MetalScrapLab
@MetalScrapLab 4 месяца назад
Interesting. I picked up bismuth as lead replacement from Jason at MBMM.
@2001pulsar
@2001pulsar 4 месяца назад
@@MetalScrapLab yes. Apparently it's the spattering of the bismuth that spreads the bead all over the cupel. Lead didn't splatter as much. Maybe lowering the temperature would help also. Lead Oxide needs 1800F or so to drive, where bismuth is around 15-1600F
@boumaarafboumaaraf8604
@boumaarafboumaaraf8604 3 месяца назад
عمل راءع .ماهو سعر الفرن من فضلك.
@gaz21lit
@gaz21lit 4 месяца назад
this is a very poor gold material and in fact much more of it is needed to get any result
@prospectorpete
@prospectorpete 4 месяца назад
Not true
@freekingawwsome
@freekingawwsome 4 месяца назад
@MetalScrapLab out got another follower nice experiment, looks like it worked well🤗
@BEETSEEKA
@BEETSEEKA 4 месяца назад
Tweaaakdrz
Далее
Turning a BLOB into PURE GOLD!
18:11
Просмотров 16 млн
Пиратские котики
00:50
Просмотров 242 тыс.
ब्रेकअप
0:16
Просмотров 5 тыс.
Can You Melt Obsidian and Cast a Sword?
14:01
Просмотров 21 млн
ROCKET that LITERALLY BURNS WATER as FUEL
19:00
Просмотров 2 млн
PCB Components Gold Recovery
11:54
Просмотров 3,1 тыс.
Damascus Steel From Milling Chips!
15:47
Просмотров 1,4 млн
Many Moving Magnets Melting Metal
20:21
Просмотров 2,9 млн
Melting silver plated items into ingots
8:39
Просмотров 18 тыс.
Copper Recovery from Fine Copper Wires Experiment
27:01